Industrial Teflon Coatings
Overview of Nyflon Layer Data
Up to 67% reduction in coefficientof friction
Corrosion resistance tested perASTM B-117
Effective deposits as low as.0002” - .0006”(5.08 to 15.24 µm )
Processing temperature< 200°F (<93°C)
400°F (204°C) max workingtemperature
Coefficient of thermal expansion13 x 10-6/°C
Applicable to nearly all basemetals
Overview of Nyflon Layer Data
Up to 67% reduction in coefficientof friction
Corrosion resistance tested perASTM B-117
Effective deposits as low as.0002” - .0006”(5.08 to 15.24 µm )
Processing temperature< 200°F (<93°C)
400°F (204°C) max workingtemperature
Coefficient of thermal expansion13 x 10-6/°C
Applicable to nearly all basemetals