Diamond Chrome Plating
A summary of XADC data for diamond chromium coatings
Surface hardness above 80Rc
10% - 67% reduction in coefficientof friction
Corrosion resistance tested toAMS 2438 per ASTM B-117
Wear resistance less than 1.2 TWIper AMS 2438
Low processing temperature<150°F (<65°C)
Typical deposit range of .0001 to.0003” (2.54 to 7.62 µm)
Effective deposit range of.000050” to .0007” (1.27 to 17.78µm)
Withstands temperatures as highas 1600°F (-240°C - 870°C)
Thermal expansion range of 2.7 -4.6 (10 ̄6/°F)