Nodular Thin Dense Chrome Plating
Overview of NTDC data for nodular thin dense chromium plating
Surface hardness up to 78Rc
10% - 67% reduction in coefficientof friction
Corrosion resistance tested toAMS 2438 per ASTM B-117
TWI as low as 0.7
Thermal expansion range of 2.7 -4.6 (10 ̄6/°F)
Density of 7.19 g/cm ̄ 3 at 20°C
Effective deposit range of.000050” to .0007” (1.27 to 17.78µm)
Withstands temperatures of-400°F to 1600°F (-240°C -870°C)
Low processing temperature,<150° F (<65°C)
Bond strength exceeding 125,000PSI
Excellent resistance to broadrange of chemicals includingacids, bases, and solvents
Overview of NTDC data for nodular thin dense chromium plating
Surface hardness up to 78Rc
10% - 67% reduction in coefficientof friction
Corrosion resistance tested toAMS 2438 per ASTM B-117
TWI as low as 0.7
Thermal expansion range of 2.7 -4.6 (10 ̄6/°F)
Density of 7.19 g/cm ̄ 3 at 20°C
Effective deposit range of.000050” to .0007” (1.27 to 17.78µm)
Withstands temperatures of-400°F to 1600°F (-240°C -870°C)
Low processing temperature,<150° F (<65°C)
Bond strength exceeding 125,000PSI
Excellent resistance to broadrange of chemicals includingacids, bases, and solvents